Relaunched 2026
A curated, not-for-profit publishing platform. Advanced Materials Letters publishes by invitation — articles from IAAM Fellows, awardees and collaborating institutions — with reading access through IAAM membership and subscription. Authors are never charged a fee.
See the access model →
Back to Browse

Graphical Abstract & Abstract

Anchor CaSO4: Dy, P is known for its dosimetric characteristics for a very long time now. In this work we have carried out a comparative study on TL intensity of CaSO4: Dy, P, Ce phosphors using two different wet chemical synthesis routes. Nobody seems to have reported this kind of study on CaSO4: Dy, P, Ce 3+ phosphors and as a result it may be regarded as something new. Phosphors were characterized by scanning electron microscopy, photoluminescence and thermoluminescence techniques. The two methods were found to drastically affect the TL intensity of CaSO4: Dy, P, Ce phosphors. The TL intensity of CaSO4: Dy, P, Ce prepared by co-precipitation method is less by a factor of 204 than the CaSO4: Dy, P, Ce phosphor prepared via acid evaporation method. Moreover, co-doping of P and Ce ions into CaSO4:Dy was observed to enhance the thermoluminescence intensity by a factor of 1.11 than the standard phosphor in case of phosphor prepared via acid evaporation method. Surface morphology resulted

How to Cite

(2013). The Influence Of Different Synthesis Routes On Thermoluminescence Of CaSO4: Dy, P, Ce Phosphors. Advanced Materials Letters, 4(5), 363-367. https://doi.org/10.5185/amlett.2012.10433